ASTM A234 WPB CS LR ELBOW 90 Degree Casting 20 Inch SCH 80
Key Specifications / Features
Model No.: DB-Carbon Steel Pipe Fittings-797 Hits: 163
China ASTM A234 WPB CS LR ELBOW 90 Degree Factory Derbo Supplies ASTM A234 WPB CS LR ELBOW 90 Degree, Casting, 20 Inch, SCH 80, PE End, Painting.
Request a quote
Share
Tags
Detail Information
Type: CS LR ELBOW 90 Degree.
Material and Grade: ASTM A234 WPB.
Size: 20 Inch, SCH 80.
Connection Way: PE End.
Manufacture Method: Casting.
Surface Treatment: Painting/Vanished/Galvanized/Coating.
Independence Inspection: Chemical Test, Mechanical Test.
Application: For Pipe Connection.
Third Party Inspection: SGS, BV, INTERNET, etc.
Packing: In Bundles/Pallet/Wooden Case or as Your Requirement.
Payment Terms: TT/LC, West Union, Paypal, O/A.
Delivery Time: 7-25 Days after Receiving the Deposit.
Material and Grade: ASTM A234 WPB.
Size: 20 Inch, SCH 80.
Connection Way: PE End.
Manufacture Method: Casting.
Surface Treatment: Painting/Vanished/Galvanized/Coating.
Independence Inspection: Chemical Test, Mechanical Test.
Application: For Pipe Connection.
Third Party Inspection: SGS, BV, INTERNET, etc.
Packing: In Bundles/Pallet/Wooden Case or as Your Requirement.
Payment Terms: TT/LC, West Union, Paypal, O/A.
Delivery Time: 7-25 Days after Receiving the Deposit.
Chemical Composition and Mechanical Property for ASTM A234 | |||||||||||
Grade |
Chemcial Composition | Mechanical Performance | |||||||||
C(Max) | Mn | P(Max) | S(Max) | Si(Min) | Cr(Max) | Mo(Max) | Ni(Max) | Cu(Max) | Tensile Strength (Min) |
Yield Strength (Min) |
|
Mpa | Mpa | ||||||||||
WPB | 0.3 | 0.29-1.06 | 0.05 | 0.058 | 0.1 | 0.4 | 0.15 | 0.4 | 0.4 | 415-585 | 240 |